Making a Spin Casting Mould/Mold with Siloset Low Temp Casting Rubber

123

 4 56 

1    Place one half of rubber mold and remove center.

2    Push masters into bottom half of mould can.

3    Dust with release agent (talc or French chalk).

4    Place mushroom in bottom half of mould. Replace top half of mould in the mold can and then can lid.

5    The prepared mould should then be placed in a rubber press @ 90-105 deg/centigrade for about 40 minutes.

6    Remove can from press and open to reveal cured  mould. Remove cured mould from can.

It is preferable to allow a cooling time before splitting mould and removing masters.